Millennium Scratch Tester

Scratch-tester Millenium

A diamond tip creates a scratch on the coating in order to evaluate its adhesion. Several parameters must be set during a scratch test. These include the force applied and the length of the scratch. This scratch is then observed using a light microscope in order to evaluate the coating resistance.

  • Coating adhesion test
  • From 0.1 N to 200 N
  • Hardness and indentation test

 

 

Exemple d'une trace réalisée à l'aide du scratchtest sur un revêtement adhérent

Example of a trace made using a scratch test on an adherent coating